Gas barrier LUMILEAD SiO

Characteristic

  1. Reduced splashing (reduced by 85%, in-house test)
  2. Refractive index of approx. 2.0-1.45 (depending on conditions)
  3. Excellent adhesion as a resin adhesion layer
Appearance

Appearance

Evaluation of the number of splashes generated at the time of film formation

Measurement conditions
Measurement device Fine particle visualization system
Film formation rate at the time of measurement 3 Å/sec
Measurement time 10 seconds
Note: This is a time period from 60 to 70 seconds after the start of vapor deposition (during which time the rate and EB output of both materials become stable).
Measurement results
Number of splashes generated at the time of film formation See the figures below.

Figure: Accumulated composite images showing the generated splashes

SURFCLEAR100/他社比較データ 耐連続磨耗性能

LUMILEAD SiO

SURFCLEAR100/他社比較データ 耐連続磨耗性能

Normal SiO

Figure: Comparison of the number of the generated splashes

SURFCLEAR100/他社比較データ 耐連続磨耗性能